Abstract

AbstractWe have studied the mechanical properties (Vickers microhardness H _V and fracture toughness K _C) of nanostructured CaO–ZrO_2–Al_2O_3 ceramic composites as dependent on the content of corundum (0 ≤ $$C_{Al_{2}O_{3}}$$ C A l 2 O 3 ≤ 25%) and the temperature of sintering (1250°C ≤ T _1 ≤ 1500°C). Optimum value of the corundum content ( $$C_{Al_{2}O_{3}}$$ C A l 2 O 3 = 5%) and optimum regime ( T _1 = 1300°C, 5 min; T _2 = 1200°C, 4 h) of two-stage sintering are established, which favor attaining the best mechanical characteristics of ceramic composites ( H _V = 12.25 GPa, K _C = 8.47 MPa m^1/2).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.