AbstractWe describe a method of obtaining ultrafine boron carbide (B_13C_2) powder using the effect of a dc electric arc on a mixture of initial reactants containing carbon and boron. A peculiarity of the proposed method is that it can be implemented using arc discharge operating in open air without any vacuum equipment and protective inert gas atmosphere. X-ray diffraction data showed that the synthesized product in the general case contained three crystalline phases: boron carbide (B_13C_2), graphite (C), and boron oxide (B_2O_3). Electron-microscopic examination showed that the average size of boron carbide particles ranged from ~50 nm to ~2 μm.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.