The hoarding rubbish synthetic plastic caused pollution and demage in life circles, to cope it can be done with synthesizing the plastic from agriculture substance or called biopolymer (bioplastic). It was that potentially as bioplastic was biopolymer from agriculture substance baggase that contain cellulose 40 %. This research aimed to determine the optimum concentration cellulose baggase in making bioplastic film with adding chitosan and sorbitol plasticizer and also to know the result of characterization film bioplastic. The steps in this research were; the extraction of cellulose, making film bioplastic, tensile strenght test and used characterization spectrofotometer FTIR. In this research showed that optimum concentration cellulose baggase in making film bioplastic was 2% with adding chitosan and sorbitol plasticizer. The optimal result of tensile strenght test was 0,089 Kgf/cm2 with elongation percent 15,90 %. The analyzing FTIR in all of variation that looked almost same with characterization with tapes -OH, -NH and C-O.