In engineering, the stress state of expanded tubes is crucial for ensuring structural integrity and preventing stress corrosion cracking. The analysis of stresses and strains in tubes subjected to mechanical expansion using an ogive bullet is essential, yet existing theoretical methods for estimating the stress distributions, especially with spherical and ogive shapes, are sparse. This study explores the expansion of 3/8 inch copper and stainless-steel tubes using an expanding bullet, where tangential and longitudinal strains are measured. A novel analytical approach is introduced to evaluate the stresses and strains, segmenting the tube into three zones, each analyzed with a distinct theory. Validation is achieved through an axisymmetric finite element model that employs a multi-linear kinematic hardening material behavior. The analytical model also estimates the expanding mandrel's push force, which is then compared with the results from numerical simulations and experimental data, showing good agreement across methods.