Percussion drilling of a Ti-based alloy with 8 ps laser pulses was investigated with emphasis on the influence of the pulse repetition rate (1–300 kHz) on the drilling process. Heat accumulation is found to be responsible for simultaneous significant rise of the average drilling rate, the occurrence of a rim around the hole entrance, as well as noticeable surface oxidation. This can be observed as soon as the repetition rate exceeds a certain critical value, which depends on the pulse energy applied. Dramatic rise of the recast layer thickness inside the growing hole was revealed for the limited range of the repetition rates around the lower boundary of the heat accumulation regime. Possible origins of this phenomenon are discussed.