Oxidation-caused electroluminescence and electrical conduction deteriorations in poly[2-methoxy-5-(2-ethylhexyloxy)-p-phenylene vinylene] (MEH-PPV) have prevented the material from being used in applications requiring air exposure. Here, we report air-stable electrical conduction in oxidized MEH-PPV layers produced by room temperature annealing of MEH-PPV thin films in air. Oxidized layers exhibit lower, but stable, conductivities. As the process is irreversible, the final conductivity is retained in vacuum, inert gas, hydrogen, and oxygen. The oxidation rates recorded at different conditions for layers of varied thickness and electrode configuration are described by a surface oxidation model. Potentials of the oxidized MEH-PPV layers in sensor technology are demonstrated.