The main failure forms of whetstones forming die is serious wear on the work face, and the boronizing technology can be used to improve the hardness and wear resistance on the work face of the whetstones forming die. In this paper, the orthogonal test was used to obtain the optimum parameters of temperature, time and the amount of addition of rare earth in the boronizing process of die. The line scan spectrum shows that there are some of elements such as B, C, Al, Cr, Si and Fe etc in boronizing layer, and their content are changed during boronizing. The microhardness of boronization layer was measured, and the result showed that maximum value of microhardness of boronizing layer appears in subsurface, not in surface, and lowers along depth of boronizing layer. By comparing different wear curve of abrasive samples with different treated, we can see that the highest wear resistance of surface is in the sample with the optimization of boronization treatment +970°C quenching and 200°C tempering; followed by quenching and tempering treatment; the lowest wear resistance of the surface is the sample without the boronizing treatment, and the rest sample are between these two samples. After optimization of boronization treatment +quenching and tempering, the lifetime of the whetstones forming die with boronizing is 3.5 times than the old one. Keywords: Boronizing; Whetstone; Forming Die