This paper summarizes the findings of an extensive research program that examined the shrinkage and creep behavior of high-strength concrete (HSC) up to a strength of 18 ksi (124 MPa). Creep and shrinkage strains of 60 specimens were monitored for up to 2 years. The variables considered in this research were the concrete compressive strength, specimen size, curing type, age of concrete at loading, and loading stress level. Findings indicate that the current American Association of State Highway and Transportation Officials' (AASHTO) LRFD Bridge Design Specifications could be used to estimate the creep coefficient and shrinkage strain of HSC up to 15 ksi (103 MPa). However, the current AASHTO LRFD specifications do not provide appropriate predictions for concrete compressive strength greater than 15 ksi (103 MPa). A revised time-development correction factor is proposed to obtain better predictions for HSC up to 18 ksi (124 MPa). For HSC compression members, the current AASHTO LRFD specifications require an excessive amount of minimum longitudinal reinforcement to account for the long-term effects due to shrinkage and creep. Based on an analysis, a new relationship is proposed for the required minimum reinforcement ratio.