Two series of samples were prepared namely Cr-Ti/MCM-41 and Cr/SiO 2-TiO 2 keeping Si/Ti mole ratio same, with different Cr loading. The physico-chemical properties of the samples were characterized by different analytical techniques such as XRD, FTIR, TEM, low temperature N 2 sorption, and UV–vis diffused reflectance spectroscopy. The impregnated TiO 2 was in anatase form. The crystallite size was determined from Scherrer equation as well as by TEM. There is a difference between the shapes of nitrogen adsorption isotherms with and without Cr-loaded Ti/MCM-41 samples. The rate of nitrogen adsorption was found to increase with decrease in Cr content at lower P/ P 0 for Cr-Ti/MCM-41 samples due to the blocking of the pores with Cr. All MCM-41 samples exhibited pore sizes from 24 nm to 32 nm. UV–vis diffused reflectance spectra of all Cr-loaded samples showed red shift of their absorption edges. Photo degradation of eosin dye was studied using visible light.