A wet solid-state method was used in this work to produce [Formula: see text]–[Formula: see text] materials. By using core-shell structure nanocubic [Formula: see text] (BMST) decorated [Formula: see text] (BBT) assemblies, a composite capacitor with improved dielectric constant and enhanced breakdown strength was successfully fabricated in contrast with the composite ferroelectric [Formula: see text]–[Formula: see text] (BBT–BST) ceramic. With increasing Mg content, the ceramic capacitors display a stronger performance in its dielectric behavior. The best dielectric properties were obtained in the composition [Formula: see text] = 0.007 with the dielectric constant above 65,000. The dielectric strength of the ceramics was measured by a withstanding voltage tester. The best dielectric strength was achieved in the composition [Formula: see text] = 0.007 with [Formula: see text] = 5.455 kV/mm.