Abstract A new kind of coating consisting of zinc oxide (ZnO)/tetracalcium phosphate (TTCP)/gelatin (Gel) on the PET woven nets is prepared chemically by the method of atomic layer deposition (ALD) and hydrothermal method. The prepared materials are confirmed by XRD and SEM. XRD results show that ZnO and TTCP are well coated on the surface of PET woven nets and ALD-assisted ZnO leads to a surprising coating adhesion of about 8 MPa. Furthermore, SEM results indicate the diameter and morphology of ZnO, TTCP and Gel of PET woven nets. And the water contact angles of PET’s surface are decreased with ZnO, TTCP and Gel of PET woven nets. Moreover, the confocal imaging of NIH3T3 cells shows that the obtained product could promote the cells proliferation, which indicates that the good biocompatibility of the prepared PET/ZnO/TTCP/ Gel woven builds a foundation for their future application. The results aim to obtain an efficient method to modify PET for fabricating an ideal artificial implant meeting the clinical needs, and imply a positive effect in promoting the compatibility of PET for enhancing graft-bone healing after implantation.

Highlights

  • We develops a novel surface modification based on our research results of the preparation about a nanoscale surface roughness ZnO film by ALD technology changes their matrix adhesion [17,18], which means that the deposition of ZnO with ALD technique is used to obtain a coating on PET woven nets

  • ZnO is deposited by ALD technology and TTCP was grown by hydrothermal synthesis, in which ZnO deposition is a key step for the strong coating adhesion between PET woven nets and coating

  • The results show that ZnO nanoparticles can cover on the surface of the PET woven nets, which is used as a medium for further TTCP growth

Read more

Summary

Introduction

Calcium phosphate ceramics is one of important biomedical bioactive ceramic materials, which composed of HA (Ca5(PO4)3(OH)), TTCP (Ca4(PO4)2O), α-TCP (Ca3(PO4)2), β-TCP (Ca3(PO4)2), and so on These calcium phosphate ceramics are always used as a surface modifier for bioactive coating on hard or soft material, including titanium alloy, stainless steel, PET, polyetheretherketone (PEEK), and so on, from some strategies of plasma spray, sol-gel, electrochemical deposition, etc. A novel PET/ZnO/TTCP/Gel woven net is prepared, which shows a good adhesion between the coating and PET woven nets of about 8 MPa. To be specific, the current study is carried out in terms of two folds: [1] to obtain an efficient method to modify PET for fabricating an ideal artificial implant meeting the clinical needs, [2] to imply a positive effect in promoting the compatibility of PET for enhancing graft-bone healing after implantation

ZnO deposition on PET woven nets
Pretreatment of PET woven nets
Characterization
Results and discussion
Conclusion
Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.