Abstract
The mechanical and fatigue properties of zirconia specimens printed by vat photopolymerization (VPP) were evaluated and compared with those of zirconia specimens milled by computer numerical control (CNC). Bar-shaped specimens were printed by stereolithography (SL) and digital light processing (DLP). CNC-milled specimens were used as control samples. The fracture toughness, hardness, and flexural strength properties of the zirconia specimens were evaluated via single edge V-notch beam tests, Vickers hardness tests, and 3-point bending tests. Dynamic fatigue tests were carried out in distilled water using a step-stress test. After static bending and dynamic step-stress testing, fractography analysis was performed. Statistical analysis was carried out to compare the fracture toughness, hardness, flexural strength, and fatigue cycle results of each group (α = 0.05). The fracture toughness values did not significantly differ among the groups (p>0.05). The flexural strength was 894.10MPa for SL, 831.46MPa for DLP, and 1140.39MPa for CNC. The flexural strength of CNC was greater than that of SL and DLP (p<0.01). The mean fatigue cycles were 23498.07 for SL, 19858.60 for DLP, and 31566.80 for CNC. The mean fatigue failure strength was 643.13MPa for SL, 530.63MPa for DLP, and 903.75MPa for CNC. The fatigue failure strength of CNC was greater than that of SL and DLP (p<0.05). Fractography analysis revealed material defects at the fracture origin for each group. A partially fused structure of the incompletely debonded resin could be observed in SL, and a porous region of incompletely sintered zirconia grains could be observed in CNC. The fracture toughness and hardness of zirconia printed by VPP are comparable to those of zirconia milled by CNC. However, zirconia milled by CNC has superior static flexural strength and dynamic fatigue resistance. Further studies are needed to explore the clinical applications of VPP-printed zirconia.
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have