Camellia oleifera shell (COS), a by-product of processing woody vegetable oil, is rich in hemicellulose and lignin. In this study, we investigated the effects of acid concentration, pretreatment temperature and reaction time on the concentration and yield of xylo-oligosaccharides (XOS) and the degree of polymerization (DP) distribution of XOS when pretreating COS with malic acid (MA). Under moderate condition (2 M MA, 120 ℃, 30 min), the maximum yield of XOS with DP 2–4 was 48.78% (based on the initial xylan) with low xylose, 5-hydroxymethylfurfural (HMF) and furfural, in which xylobiose (X2), xylotriose (X3) and xylotraose (X4) concentrations were 5.22 g/L, 2.75 g/L and 2.91 g/L, respectively. In addition, acid-insoluble lignin (AIL) in the residue after MA pretreatment and milling wood lignin (MWL) were mainly composed of guaiacyl and syringyl. AIL has higher thermal stability than MWL, which can be the stabilizer for producing flame-resistant materials.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call