Abstract

Tricalcium silicate (C3S), the major phase of cement-based materials, contains naturally a few hundred parts per million of heavy metals. An X-ray absorption spectroscopy (XAS) study at the Zn K-edge has been carried out to elucidate the binding mechanisms of Zn by calcium silicate hydrates, which is important to predict the long-term behavior of Zn. At low concentration, under the threshold of precipitation of the oxide, oxy hydroxide, and calcium zinc hydroxide, no retardation of the hydration of the C3S has been observed for C3S doped with Zn. A previous 29Si NMR (Moulin, I.; Stone, W. E. E.; Sanz, J.; Bottero, J.-Y.; Mosnier, J−Y.; Haehnel, C. Langmuir 1999, 15, 2829−2835) study has demonstrated that the structure of the hydrated C3S (called C-S-H for calcium silicate hydrates) does not change if Zn is present initially or not. XAS experiments have shown that Zn tetrahedra are incorporated within the matrix of C-S-H and linked directly at the end of the silicate chains through Zn−O−Si bonds. The Zn−Si distance is ≈3.1 Å. Extended X-ray absorption fine structure results have been confirmed by ab initio calculations including multiple scattering.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.