Contact wetting angle of Pd43Ni10Cu27P20, Pt57.5Cu14.7Ni5.3P22.5, Au49Ag5.5Pd2.3Cu26.9Si16.3, and Zr57Nb5Cu15.4Ni12.6Al10 bulk metallic glass forming alloys have been determined on materials that are used in micro and nano fabrication. Employing the sessile drop technique at a temperature above the corresponding melting temperatures, three kinds of wetting behaviors are observed, spanning from θ ≈ 140°, over neutral wetting, θ ≈ 80°, to almost complete wetting, θ < 5°. The origin for complete wetting is the formation of an interface phase promoting wetting. Estimations of the contact wetting angles are presented for temperatures in the supercooled liquid region where micro and nano fabrication is typically carried out. Consequences of the observed wetting behaviors for nanoforming are discussed.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.