Abstract
Fossil fuel will continue to be the major source of energy for the foreseeable future. To meet the demand for clean and affordable energy, an increase in the operating efficiency of fossil fired power plants is necessary. There are several initiatives worldwide to achieve efficiencies >45%HHV through an increase in steam temperature (700–760°C) and pressure (27.6–34.5 MPa). Realising this goal requires materials with excellent creep rupture properties and corrosion resistance at elevated temperatures. Two previous papers addressed the welding and weldability of ferritic and austenitic stainless steels. Welding and weldability of nickel based alloys will be discussed in a two-part paper. In this paper, the primary focus will be on the behaviour of candidate nickel based alloys that are being proposed in advanced ultrasupercritical power plants and with regard to weldability (Part I) and cross-weld creep performance (Part II).
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.