Abstract
Fossil fuel will continue to be the major source of energy for the foreseeable future. To meet the demand for clean and affordable energy, an increase in the operating efficiency of fossil fired power plants is necessary. There are several initiatives worldwide to achieve efficiencies >45% higher heating value (HHV) through an increase in steam temperature (700 to 760°C) and pressure (27.6 to 34.5 MPa). Realising this goal requires materials with excellent creep rupture properties and corrosion resistance at elevated temperatures. In order to accomplish this, three classes of materials have been identified: creep strength enhanced ferritic steels, austenitic stainless steels and nickel base superalloys. Although new alloys have been designed and developed to meet this need, welding can have a significant and often detrimental effect on the required mechanical and corrosion resistant properties. Two previous papers addressed the welding and weldability of ferritic and austenitic stainless steels. Welding and weldability of nickel base alloys will be discussed in a two part paper. In this paper, the primary focus will be on the fundamentals of welding and weldability of Ni base superalloys.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.