Abstract
Abstract A modified mixing and casting procedure was used for the preparation of Al-1.2 Si-0.8 Fe–Gr composite (wt.%). Graphite and gray cast iron powders were blended and dispersed in Al-1.2 Si matrix alloy melt and poured in a cast iron mould. Gray cast iron powder worked as carrier for graphite particles. The presence of graphite improves the ultimate tensile strength, tensile and compressive stress but beyond 1 % of graphite all properties deteriorate. However, hardness continuously increases and percentage elongation reduces with graphite. In wear studies, different mechanisms: mild-oxidative, oxidative-metallic and severe-metallic, are operative in the different combinations of sliding velocities and applied loads.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.