Abstract

The water sorption and solubility characteristics of three contemporary methacrylate resin-based endodontic sealers, EndoREZ, Epiphany, and InnoEndo, were compared with those obtained from Kerr EWT, Ketac-Endo (positive control), GuttaFlow, and AH Plus (both negative controls). Ten disks of each material were dehydrated in Drierite for 24 h and weighed to constant dry mass. They were placed in water and weighed periodically until maximum water sorption was obtained. The disks were dehydrated again to determine their mass loss (solubility) at equilibrium. Epiphany exhibited the highest apparent water sorption (8%) followed by Ketac-Endo (6.2%), InnoEndo (3.4%), EndoREZ (3.0%), AH Plus (1.1%), GuttaFlow (0.4%), and Kerr EWT (0.3%). Significantly higher solubility (3.5-4%) were observed for all three methacrylate resin-based sealers and Kerr EWT (3.95%), compared with Ketac-Endo (1.6%), AH Plus (0.16%), and GuttaFlow (0.13%). American Dental Association specifications require<3% solubility for endodontic sealers. Only Ketac-Endo, AH Plus, and GuttaFlow met that criterion.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.