‘Wealth from Waste’ is an emerging concept, since it leads an effective waste treatment and waste recyclability. On the other hand, cost effective production iron oxide (IO) nanomaterials is still needed to develop, owing to their wide applications. Herein, we proposed a simple direct calcination method to prepare porous IO (Fe3O4 and Fe2O3) nanomaterials from waste toner powder. Characterization techniques reveal that a structural change happened from Fe3O4 to γ-Fe2O3 and γ-Fe2O3 to α-Fe2O3 at the calcination temperature of 500 °C and 700 °C respectively. Consequently, optical (band gap) and magnetic parameters of IO samples were significantly varied. The pigment characteristics of the IO samples were evaluated using Commission Internationale de l’Eclairage (CIE) analysis. IO900 sample has shown good brown-red coloration (L* = 43.11, a* = 13.26 and b* = 5.69) and it also exhibited good stability in acidic and basic conditions. Practical applicability of IO pigments were also tested by mixing with plaster of paris (PP) powder. Further, porous IO samples were also used as catalysts in the reductive degradation of methyl orange (MO) dye in presence of excess sodium borohydride (NaBH4). IO, prepared at 900 °C exhibited ∼99.9% reduction efficiency within 40 min. Recycling experiments indicated that IO900 possess good stability up to seven cycles. The present porous IO samples will become potential in pigment and environmental remediation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.