Cyclic voltammetry was used to study the formation of graphite oxide film on the surface of rotating-disc glassy carbon electrodes. The film was formed by continuous potential cycling in phosphate buffer electrolyte. It was found that when cycling between the totally oxidized and totally reduced potential ranges (between + 2.3 and −1.2V vs. SCE), well-shaped redox peaks were obtained. Typical voltammograms comprised one cathodic and two anodic waves, where the anodic waves were directly related to the oxidation of surface-bound products associated with the cathodic process. All three processes were pH dependent. Freshly formed surface graphite oxide films were not stable and would undergo transformation to give the stable state upon potential cycling between potentials ± 1.0V. The ultimate stable voltammograms were characterized by two electrode processes. The quasi-reversible process involved surface quinone-like functional groups, while the other irreversible process might be related to the uptake and release of hydrogen ions at the porous graphite oxide film.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.