Abstract
Vertically aligned TiO2/ZnO nanotube (NT) arrays were developed for application to photoanodes in mesoscopic solar cells. By a two-step anodic oxidation, vertically aligned TiO2 NT arrays with highly ordered surface structure were prepared, followed by deposition of a ZnO shell with a precisely controlled thickness using atomic layer deposition (ALD). When applied to a photoanode of dye-sensitized solar cells (DSSCs), the photovoltage is gradually enhanced as the ZnO shell thickness of the TiO2/ZnO NT electrodes is increased. Furtheremore, the electron lifetime in photoanodes is significantly enhanced due to the ZnO shell, which is examined by open-circuit voltage decay (OCVD) measurement. Photocurrent density-voltage (J-V) curves under the dark condition and OCVD spectra reveal that a negative shift in TiO2 conduction band potential and an energy barrier effect owing to the ZnO shell concurrently contribute to the enhancement of VOC and electron lifetime.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.