Abstract

In this work, thealkaline roasting and sulfuric acid leaching processes were employed to extract vanadium from the magnetite ore of Saghand mine in central Iran. The response surface methodology based on the central composite design model was applied to optimize the parameters involved in the processes. The studied roasting parameters were temperature (900-1100 °C), sodium carbonate percentage (30-50 wt%), and time (1-3 h). In addition, the studied leaching factors included temperature (70-90 °C), liquid-to-solid ratio (L/S) (5-20 mL/g), sulfuric acid concentration (2-6 M), and time (3-6 h). Under the optimal conditions, the values for temperature, time, and sodium carbonate amounted to 1010 °C, 2.1 h, and 41 wt%, respectively, for the roasting process, while the values for temperature, L/S, sulfuric acid concentration, and time for the leaching process were estimated to be 85 °C, 12.4 mL/g, 4.25 M, and 4.7 h, respectively. Under these conditions, about 83.8 ± 0.9% of vanadium was leached from the magnetite ore.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.