Abstract

Compared with traditional sodium or calcification roasting process for vanadium extraction from raw vanadium slag (V-slag), ammonium sulfate (AS) roasting could reduce about 470 °C roasting temperature and avoid Cl2, HCl, sodium-containing waste-water and waste gypsum discharging. To reduce the amount of AS added in vanadium extraction process, an efficient AS two-stage cyclic roasting and acid leaching process was proposed. The result of TG analysis indicates V-slag could be decomposed in 275–380 °C using AS roasting process. Using 2.03:1 total mass ratio of AS to V-slag, 90.86% V and 80.54% Ti could be extracted after 380 °C roasting for 30 min and 8% initial concentration of H2SO4 leaching at 70 °C for 100 min. XRD analysis indicates V-containing spinel phase in the 1st stage leaching residue would be efficiently decomposed by the cyclic two-stage roasting and leaching process. Furthermore, the valence of V(III) in raw V-slag was not changed after the 1st AS roasting stage, but a part of V(III) in the 1st leaching residue was oxidized to V(V) after 2nd roasting process.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.