Abstract

Vacancy-related defect profiles have been measured for La0.5Sr0.5CoO3/(Pb0.9La0.1)(Zr0.2Ti0.8)O3/La0.5Sr0.5CoO3 ferroelectric capacitors using a variable-energy positron beam. By varying the layer thickness and the postgrowth processing in a reducing ambient, a capacitor showing oxygen deficiency dominantly in the top electrode and one with deficiency in both electrodes were produced. The capacitor with an asymmetric defect profile showed a voltage offset polarization–voltage hysteresis loop, that with a symmetric distribution of vacancy-related defects showed no offset. These results are discussed in the context of current models for imprint.