Abstract

his paper studies the feasibility of preparation high strength fired bricks from iron tailings with addition of clay and coal gangue. The results indicated that the optimum conditions were found to be that the hematite tailings content were 35%–50%; the firing temperature was 1000 °C. Under these conditions, the mechanical strength, the water absorption and the bulk density of the fired bricks were 21.17–26.14 MPa, 14.55–15.47% and 1.648–1.629g/cm3, respectively, these were well conformed to standards MU20 of Chinese Fired Common Bricks Standard (GB/T5101-2003).The phase composition and microstructure of the fired specimen were characterized by XRD and SEM. The results showed that the major crystalline phases present in fired brick were quartz, albite, amphibole, hematite and muscovite, and glass phase encapsulated and cement the crystalline phases forming strong entirety which promoted the strength of bricks.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call