WO3, activated by 1% Pt or 1% Pd, was deposited by radio frequency co-sputtering process. The as-sputtered films were thermally-treated at 450°C for 24h after co-sputtering. The microstructure, crystal structure and chemical composition of the as-sputtered and thermally-treated films were analyzed by SEM, XRD and XPS. The sensing characteristics of the Pt or Pd activated WO3 films, as well as the pure WO3 films, were characterized with 25-200ppm H2, 25-200ppm CO and 0.62-5ppm NH3 at 50-300°C in air with different humidity.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.