Abstract

The using of bottom ash and tailing were by product from Mae Moh coal fired power plant as mine backfill. Laboratory was investigated the chemical, physical and mechanical properties of backfill containing bottom ash, tailing and cement. Using cast of backfill materials to test the ability of compressive strength in box size 5×5×5 cm. Four different types of backfill that portland cement type 1 was replaced by bottom ash, in the proportion of percent 5, 10, 15 and 20 by weight uncured and cured in water for 7 and 28 days. Backfill materials characterization bottom ash have been examined in grain size distribution, chemical composition analyzed by X-ray fluorescence (XRF) of backfill material. For the mechanical property was test by uniaxial compressive strength machine. The result was found that mixing ratio of bottom ash can be used as backfill material ranging from 15-20 % by weight. The mechanical property of backfill mixture suitable for use with compressive strength from 6.4-19.7 MPa and cured in water 28 days was maximum compressive strength.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.