Rutile (TiO2) is heavily used in pigments and colorants, and the most abundant source of rutile is ilmenite. Upon oxidation of ilmenite, rutile can be formed with modest energy consumption; furthermore, after leaching, only a few byproducts are formed. Unfortunately, one drawback is the necessarily long oxidative process of typically used methods. In this study, we show that a fluidized bed reactor can be used to oxidize ilmenite ore to rapidly form rutile and pseudobrookite (Fe2TiO5) phases. Ilmenite was oxidized with 5vol% O2 in Ar at temperatures of 1173 K or 1223 K and subsequently leached using a diluted H2SO4 solution to dissolve the pseudobrookite phase. The effects of acid concentration, temperature, and cooling rate after oxidation were investigated. We show that the ilmenite was rapidly oxidized to form rutile and pseudobrookite phases at 1173 and 1223 K in a 5vol% O2/95vol% Ar environment within 40 min. The final maximum rutile yield was 84.2mol% after leaching in (1 + 1) H2SO4 solution at 393 K for 12 h.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call