The transformation of vitrified waste, such as bottom ash from municipal waste incineration, into cellular glass-ceramics is convenient, if the additional processing is simple and inexpensive. The present paper aims at presenting a possible route to achieve this goal, based on the recently proposed mechanical foaming of alkali-activated suspensions of waste glass powders, followed by sinter-crystallization at moderate temperatures (from 800 to 900 °C). Compared to previously studied glasses, in this experiment bottom ash-derived glass suspensions underwent progressive hardening at low alkali molarity and in limited times. The firing did not alter the open-celled structure that had developed upon low temperature foaming, owing to a significant crystallization. With an overall porosity of 80%, the optimized foams exhibited a remarkable compressive strength (>6 MPa). Finally, the process had no negative impact on the leaching of toxic elements, which remained well below the thresholds for inert materials.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call