Abstract

The production of Gd5(Si,Ge)4 compounds in reduced dimensionality, through pulsed laser deposition (PLD), have shown their potential for practical applications. Here, we present nanoparticles ranging from 10 to 27 nm of average particle size of Gd5(SixGe1−x)4, with x = 0, 0.45 and 0.60, obtained using an Nd:Yag (1064 nm) and an Excimer KrF laser (248 nm). Synchrotron X-ray Diffraction measurements revealed a reduced unit cell volume in comparison to their bulk counterpart. The x = 0 sample presented a ∼1.99% reduction while x = 0.45 composition, a shrinkage of ∼1.81% on the unit cell volume that are a result of a structural change to a Gd5Si4-type structure [O(I)]. In contrast, x = 0.60 nanoparticles conserve the bulk crystal structure with ∼ 0.95% of volume shrinkage. As a consequence, there is a change on the magnetic transition order from a first to a second one for all nanostructures followed by a magnetocaloric response reduction. These observations unveil a direct correlation between the bulk compressibility values and the unit cell shrinkage, suggesting that the rise of a surface stress plays a major role on the particle and unit cell dimensions.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.