A novel method, Flash Spark Plasma Sintering (FSPS), combining flash sintering and electric field assisted sintering was used to densify B4C ceramics. B4C powder was densified up to 99.2% in 1min with limited grain size increase at 1931°C under an applied pressure of 15.3MPa. TEM analysis of the grain structure of the resulting ceramics suggests that the Joule heating and sparking initiated by the pulsed current are highly localized to particle interfaces and contribute significantly to the character of densification. We show that plastic deformation under high current and low pressure is the dominant densification mechanism.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.