Abstract

This study evaluated the repair bond strength of Estenia composite. Disk specimens of a dentin material were conditioned with varying combinations of silane primer (Add-on Primer, Clearfil Porcelain Bond Activator, Clearfil Porcelain Bond Activator + Clearfil Mega Bond-Primer, Porcelain Liner M, and unprimed) and bonding agent (Clearfil Mega Bond-Bond, Modeling Liquid, Stain Diluent, and no bonding agent). After photopolymerization of the enamel material placed on each surface, the specimens were either wet- or dry-stored at 37 degrees C for 24 hours. Average shear bond strength varied from 24.9 to 61.4 MPa, where the Clearfil Porcelain Bond Activator + Clearfil Mega Bond-Bond group and the Add-on Primer + Modeling Liquid group showed the greatest bond strength for dry and wet conditions respectively. To achieve reliable bond strength between layers of Estenia composite, it is highly recommended to use specific combinations of silane primer and bonding agent.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.