Abstract
We demonstrate electrical tunnel spin injection from a ferromagnet to graphene through a high-quality Al2O3 grown by atomic layer deposition (ALD). The graphene surface is functionalized with a self-assembled monolayer of 3,4,9,10-perylene tetracarboxylic acid (PTCA) to promote adhesion and growth of Al2O3 with a smooth surface. Using this composite tunnel barrier of ALD-Al2O3 and PTCA, a spin injection signal of ∼30Ω has been observed from non-local magnetoresistance measurements at 45K, revealing potentially high performance of ALD-Al2O3/PTCA tunnel barrier for spin injection into graphene.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.