Abstract
Si wafers implanted at 5, 15, and 50 keV with different BF2+ doses and next annealed at 945 °C for 45 s, were studied by means of x-ray triple crystal diffraction, x-ray standing wave, and transmission electron microscopy methods. Due to the implantation energies used, very narrow subsurface regions with a depth ranging from a few tens of nanometers to a few nanometers were damaged. By fitting the diffraction curves and using the information obtained from the photoelectrons emitted by the x-ray standing wave field, it was possible to determine the most appropriate strain and damage profiles versus depth within the disturbed region of the crystal. The above results made it possible to find: (i) the distribution of interstitial ions produced during the implant processes; (ii) the depth of amorphization of the implanted regions at the highest doses; and (iii) the appearance of extended defects (dislocation loops band) at the amorphous/crystal interface during the restoration of the lattice by the annealing process. Transmission electron microscopy investigations and electrochemical capacitance–voltage profiling measurements were made on several annealed samples and the results obtained by the x-ray diffraction and standing wave methods were confirmed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.