Abstract
The tribological properties on the friction and wear properties of cast iron CrMo and 38CrMoAlA materials under the load, temperature, sliding speed were investigated on a MMW-1 high temperature friction-wear tester. The worn surface morphology was observed and analyzed by scanning electron microscope (SEM). The results show that considering the impact of the three factors, the conclusion was that larger influence on adhesive wear was mainly test temperature and sliding speed, the influence of the load was minimal. The main influence of test temperature and sliding speed was adhesive wear. The abrasive wear and plough cut wear were mainly caused by the load. When the synergy of the load, temperature and sliding speed reach a certain condition.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.