Abstract

The aim of this study is to compare the tribological characteristics of OPF/E and KF/E composites in terms of fibre composition and temperature. A pin sample with a diameter of 10mm was made using the hot compaction technique. The dry sliding test was performed using a pin-on-disc tribometer. Increasing the temperature resulted in increased wear and decreased friction coefficient for both composites. The mild-severe wear transition of OPF/E accelerated with fibre composition although it produced a lower wear rate than KF/E at high-temperatures. In addition, the wear mode map for both OPF/E and KF/E composites has been proposed and addressed in this paper based on wear rate values. This mild-severe wear transition has been further confirmed by worn surface morphology.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.