The transformation of conventional binder and grout into high-performance nanocarbon binder and grout was evaluated in this investigation. The high-performance nanocarbon grout consisted of grey cement, white cement, lime, gypsum, sand, water, and graphite nanoplatelet (GNP), while conventional mortar is prepared with water, binder, and fine aggregate. The investigated properties included unconfined compressive strength (UCS), bending strength, ultrasound pulse analysis (UPA), and Schmidt surface hardness. The results indicated that the inclusion of nanocarbon led to an increase in the initial and long-term strengths by 14% and 23%, respectively. The same trend was observed in the nanocarbon binder mortars with white cement, lime, and gypsum in terms of the UCS, bending strength, UPA, and Schmidt surface hardness. The incorporation of nanocarbon into ordinary cement produced a high-performance nanocarbon binder mortar, which increased the strength to 42.5 N, in comparison to the 32.5 N of the ordinary cement, at 28 days.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.