Abstract
AbstractA new atomic layer deposition (ALD) process for nanocrystalline tin dioxide films is developed and applied for the coating of nanostructured materials. This approach, which is adapted from non‐hydrolytic sol‐gel chemistry, permits the deposition of SnO2 at temperatures as low as 75 °C. It allows the coating of the inner and outer surface of multiwalled carbon nanotubes with a highly conformal film of controllable thickness. The ALD‐coated tubes are investigated as active components in gas‐sensor devices. Due to the formation of a p‐n heterojunction between the highly conductive support and the SnO2 thin film an enhancement of the gas sensing response is observed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.