Abstract
A new atomic layer deposition (ALD) process was applied for the homogeneous coating of carbon nanotubes with vanadium oxide. It permits the coating of the inner and outer surface with a highly conformal film of controllable thickness and, hence, the production of high surface area hybrid materials at a so far unprecedented quality. The ALD-coated tubes are used as active component in gas-sensing devices. They show electric responses that are directly related to the peculiar structure, i.e., the p-n heterojunction formed between the support and the film.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.