Abstract
The removal of toxic heavy metal ions from water resources is crucial for environmental protection and public health. In this study, we address this challenge by developing a surface functionalization technique for the selective adsorption of these contaminants. Our approach involves atomic layer deposition (ALD) followed by vapor-phase silanization of porous substrates. We utilized porous silica gel powder (∼100 μm particles, 89 m2/g surface area, ∼30 nm pores) as an initial substrate. This powder was first coated with ∼0.5 nm ALD Al2O3, followed by vapor-phase grafting of a thiol-functional silane. The modified powder, particularly in acidic conditions (pH = 4), showed high selectivity in adsorbing Cd(II), As(V), Pb(II), Hg(II), and Cu(II) heavy metal ions in mixed ion solutions over common benign ions (e.g., Na, K, Ca, and Mg). Langmuir adsorption isotherms and breakthrough adsorption studies were conducted to assess heavy metal binding affinity and revealed the order of Cd(II) < Pb(II) < Cu(II) < As(V) < Hg(II), with a significantly higher affinity for As(V) and Hg(II) ions. Time-dependent uptake studies demonstrated rapid removal of heavy metal ions from aqueous environments, with Hg(II) exhibiting the fastest adsorption kinetics on thiol-modified surfaces. These findings highlight the potential of ALD and vapor-phase silanization to create effective adsorbents for the targeted removal of hazardous contaminants from water.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.