Abstract
AbstractThe effect of specimen thickness on the creep response of Ni-based single-crystal superalloy DD6 was investigated. With the thickness of 0.3 mm, 0.6 mm and 1.2 mm, a series of thin-wall specimens were tested in this paper respectively at 760℃, 980℃ and 1,100℃. Under the conditions of lower temperatures and higher stresses, the creep life of thin-wall specimens increases with the increase of δ, but it is almost equal under higher temperatures and lower stresses conditions. Compared with the standard specimens, an obvious reduction (about 60%) of creep life of the thin-wall specimens was found at 760℃, whereas it is almost the same at 980℃ and 1,100℃. Therefore, obvious thickness effect is prone to lower temperature and higher stress. The thickness effect is a comprehensive effect, which is caused by fracture mode, the degree of necking, the shape and quantity of creep cavities, oxide thickness, etc. Under each condition, an increased thickness resulted in increased creep strain to rupture.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.