Abstract

This paper reports the thickness and temperature dependence of the conductivity for dc glow-discharge amorphous silicon (a-Si : H) films. It is found that the kink temperature, at which an abrupt change of activation energy occurs, rapidly increases for the samples thinner than 0.24 μm and that this phenomenon can be used to determine the depth of surface band bending.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.