Abstract

AbstractThe effect of soft segment molecular weight and chemical structure on the morphology and final properties of segmented thermoplastic polyurethanes containing various hard segment contents has been investigated from the viewpoint of the degree of microphase separation. Vegetable oil‐based polyesters and corn sugar‐based chain extender have been used as renewable resources. The synthesis has been carried out in bulk without catalyst using a two‐step polymerization process. Physicochemical, thermal and mechanical properties, and also morphology, have been studied using Fourier transform infrared spectroscopy, differential scanning calorimetry, dynamic mechanical analysis, atomic force microscopy, X‐ray diffraction and mechanical testing. Chemical structure and molecular weight of polyols strongly affect the properties of the synthesized segmented thermoplastic polyurethanes. An increase in soft segment molecular weight leads to an increase of the degree of soft segment crystallinity and microphase separation, thus giving enhanced mechanical properties and higher thermal stability. Copyright © 2012 Society of Chemical Industry

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.