A thermopile sensor composed of 196 pairs of p–n thin film legs was processed on a glass substrate by using successive electrodeposition of the n-type Bi–Te and the p-type Sb–Te thin films. The 5.3-μm thick Bi–Te film, electrodeposited at a constant voltage of -50 mV in the 50-mM electrolyte with the Bi/(Bi + Te) mole ratio of 0.5, exhibited a Seebeck coefficient of -67 μV/K. The 5.2-μm thick Sb–Te film, electrodeposited at a constant voltage of 20 mV in the 70-mM solution with the Sb/(Sb + Te) mole ratio of 0.9, possessed a Seebeck coefficient of 63 μV/K. The thermopile sensor exhibited the sensitivities of 13.1 mV/K with temperature differences smaller than 9 K and of 27.3 mV/K with temperature differences larger than 9 K respectively, across the hot and cold ends.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.