Abstract Thermal-swing extraction of CdII with a thermosensitive gel, poly(N-isopropylacrylamide) (NIPA) crosslinked with an encapsulating ligand, N,N,N′,N′-tetrakis(4-propenyloxy-2-pyridylmethyl)ethylenediamine (TPPEN), was examined. CdII was extracted in the gel swollen at 5 °C and released from the gel shrunken at 40 °C. The difference in the distribution ratios of CdII between these temperatures was more than 30 times.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.