The behaviour of two Nicalon/calcium aluminosilicate ceramic composite laminates (a (±45°)3s and a plain-weave woven) under conditions of thermal shock has been studied. Test specimens heated at various temperatures were quenched into room-temperature water. This was followed by detailed damage characterisation. In addition, post-shock mechanical properties were assessed by tensile tests (for the woven laminate) and flexural tests (for both laminates). Both materials were found to have comparable thermal shock resistance. Crack morphologies comprised matrix cracks of various orientations that exhibited similar characteristics to those described for thermally shocked cross-ply laminates with the same constituents, but cracking was found to be less widespread in the woven laminate. Fibre breaks were also detected on the woven material when high-temperature degradation of the fibre–matrix interface was present. A gradual reduction in properties (stiffness, proportional limit stress, fracture strength) of thermally shocked specimens was identified, which began at larger shocks than those at which thermal shock damage initiated. This was attributed to the extension of some matrix cracks into the bulk of material.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call