Abstract

The thermal properties of two different compositions (Te 12 and 17at.%) of In–Sb–Te, obtained by metalorganic chemical vapour deposition, were investigated by the 3 ω method. The thermal conductivity of these chalcogenides, of interest for phase change memory applications, was found to decrease with increasing tellurium content. Thermal treatment at 480°C of these materials caused an increase of their crystallinity and improved the thermal conductivity. However, this effect was more marked in the Te-poor composition than in the Te-rich one. In addition, the thermal boundary resistance between In–Sb–Te and various capping dielectrics (SiO2, Si3N4 and Al2O3) was measured and it was found to be closely correlated to the interlayer roughness, as indicated by X-ray reflectivity. In this regard, silicon oxide and alumina yielded a smoother and less resistive interface with In–Sb–Te than silicon nitride.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.