Abstract

Abstract. The natural rubber latex (NRL) concentrate was mixed with 10~50 parts per hundred rubber (phr) of methyl methacrylate-grafted-natural rubber latex having a methyl methacrylate content of 49% (MGL49), prevulcanized, and then cast to obtain prevulcanized NRL/MGL49 films. The leached films of prevulcanized NRL/MGL49 were aged in an hot-air oven for comparison of the mechanical properties before and after aging, whereas the thermal decomposition of these films in an atmosphere of air was carried out in a thermo-gravimetric analyzer, and the films were also immersed into water to obtain water absorption. Results showed that the incorporation of MGL49 improved the thermal-oxidative aging resistance of natural rubber latex film when the MGL49 content was less than 50 phr, the water absorption increased with the increment of MGL49 content, and the NRL/MGL49 film containing 10phr of MGL 49 has a best thermal-oxidative stability and highest water absorption also.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call