Abstract

AbstractBy introducing high precision sample alignment technique, repeatability of incident angle to the sample surface for x-ray reflectivity (XRR) measurement is achieved to be within 0.3 arcsec. As a result, film thickness and density are possible to be measured repeatability within 0.03% and density within 0.26%. This accuracy realized to detect very small change of thermal expansion of thin films. The coefficient of thermal expansions (CTE) for porous low-k films deposited by CVD method were measured up to 400°C. The obtained values are in the range from 40 to 80 x10-6 K-1 and they are very large compare to that of copper (16-20 x10-6 K-1).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.